subject
Engineering, 29.10.2020 17:00 amandasantiago2001

For a steel alloy it has been determined that a carburizing heat treatment of 10 h duration at 753°C will raise the carbon concentration to 0.50 wt% at a point 3.3 mm from the surface. Estimate the time necessary to achieve the same concentration at a 5.6 mm position for an identical steel and at a carburizing temperature of 1060°C. Assume that D0 is 3.2 × 10-5 m2/s and Qd is 104 kJ/mol.

ansver
Answers: 1

Another question on Engineering

question
Engineering, 03.07.2019 14:10
Line joining liquid phase with liquid and solid phase mixture is known as: a) liquidus b) solidus c) tie line d) none of the mentioned
Answers: 2
question
Engineering, 03.07.2019 19:30
When using the ohmmeter function of a digital multimeter, the leads are placed in what position relative to the component being tested? a. parallel b. control c. series d. line
Answers: 3
question
Engineering, 04.07.2019 19:10
The proportional limit is always greater than the yield strength for a material. a)-trune b)- false
Answers: 3
question
Engineering, 04.07.2019 19:10
A)-in the process of engineering design, explain the contribution of material selection. b)- explain the procedure of synthesis as is employed in engineering design. c)- is there any relationship between ergonomics and engineering design? explain. d)- safety consideration in engineering design includes human, product and the enviroment . explain how safety will be incorporated into the design?
Answers: 3
You know the right answer?
For a steel alloy it has been determined that a carburizing heat treatment of 10 h duration at 753°C...
Questions
Questions on the website: 13722360